Old 6th April 2008, 05:45 PM   #16
katana
Member
 
katana's Avatar
 
Join Date: Jan 2006
Location: Kent
Posts: 2,658
Default

Quote:
Originally Posted by kronckew
flashing is the thin 'feathers' of metal that ooze from the body of the item into the thin joint where the two mold halves meet, it's usually cut or ground back, either resulting in the distinctive mold lines around the join, or if properly finished, you'll not see it at all... if you've ever done plastic airplane models, you'll remember the thin plastic you trimmed off the parts to get them to fit. flashing. there may be some in the inside of the rings where it hasn't been cleaned out fully.

Thanks Kronckew ,
........so nothing to do with with raincoats then ...



I found this regarding early moulds for bronze .....interestingly it seems that after casting, 'hammer work' can improve the finished article...

http://ads.ahds.ac.uk/catalogue/adsd...32_039_041.pdf

http://www.darwincountry.org/explore/003450.html


Regards David

Last edited by katana; 6th April 2008 at 06:13 PM.
katana is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 04:43 PM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.