#21 | |
Member
Join Date: Mar 2006
Location: Sturgeon Bay, Wisconsin
Posts: 163
|
![]() Quote:
The "normal" type I use is Nantan and Campo. The nantan has almost pure nickel srips inside and is rusted in many places...it is good for melting, but I think simply folding it in would be problematic for the first five wleds or so. Alan, "low tech" is good till you have to make a living. I struggled with this for years before I made the leap to larger tools. I work alone and have a wide range of jobs. In the past I have forged knives using a granite hammer and anvil and forge welded with a box bellows and charcoal whith a forge of mud...it works, but I can not make railings that way. If someone wants a traditional piece than I do it as close as I can recreate, but few wish to pay the added expense. Ric |
|
![]() |
![]() |
|
|