Quote:
Originally Posted by lemmythesmith
Hi Ric, what kind of meteorite is that? Is it the Nantan? Has it turned to a kind of haematite? I've seen those on E-Bay, if it was one of those just wondering if you broke it up did it have any cracks or fissures inside? Might be an interesting ukiran material. Probably a wee bit heavy though!
That particular piece in the photo was supplier by a client..it was a Russian fall, but I do not remember the name.
The "normal" type I use is Nantan and Campo. The nantan has almost pure nickel srips inside and is rusted in many places...it is good for melting, but I think simply folding it in would be problematic for the first five wleds or so.

Alan,
"low tech" is good till you have to make a living. I struggled with this for years before I made the leap to larger tools. I work alone and have a wide range of jobs. In the past I have forged knives using a granite hammer and anvil and forge welded with a box bellows and charcoal whith a forge of mud...it works, but I can not make railings that way.
If someone wants a traditional piece than I do it as close as I can recreate, but few wish to pay the added expense.

Ric