#1 |
Member
Join Date: Nov 2010
Location: Wirral
Posts: 1,204
|
![]() |
![]() |
![]() |
![]() |
#2 |
Member
Join Date: Apr 2005
Posts: 3,255
|
![]()
That may be due to lots of mineral filler.
The developing smoke should have some kind of plastic smell though (vs. the smell at a dentist when drilling a tooth)... Regards, Kai |
![]() |
![]() |
![]() |
#3 |
Member
Join Date: Nov 2010
Location: Wirral
Posts: 1,204
|
![]() |
![]() |
![]() |
![]() |
#4 |
Member
Join Date: Nov 2023
Location: France
Posts: 13
|
![]()
hello,
first of all, the tusk should be hollow at that point (base!). And the little holes give it away, as a resin copy. They are due to air bubbles. Something you get if you do not pay attention on the job... So in fact it is; a sloppy made copy... |
![]() |
![]() |
![]() |