Quote:
Originally Posted by estcrh
I think sand casting would be the method for making an iron / steel hilt, lost wax is good for metals with a low melting point. With sand casting I do not think you would get as much detail as you would with lost wax.
Exactly! That's why after casting, the Iron hilts need to be processed to give them the desired finish and detail.
mariusgmioc is offline   Reply With Quote
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 12:09 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.