Muriatic is a 33% dilution of hydrochloric acid, the main drawback/risk of using it is its propensity to form an acid fog that will coat every bit of steel (even stainless) in the room/building with a layer of very active rust, do not play with it in the same building your collection is housed in!!
I once got to check out 12 brand-new stainless elevators that needed to be replaced when the flooring contractor washed the newly-laid granite floor with muriatic to remove grout residue... expensive!
Jeff Pringle is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +1. The time now is 05:17 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
Posts are regarded as being copyrighted by their authors and the act of posting material is deemed to be a granting of an irrevocable nonexclusive license for display here.