#11 | |
Member
Join Date: Jan 2005
Location: Kansas City, MO USA
Posts: 312
|
![]() Quote:
I understand, I think you are Ok with the metallic part of the Nantan. There shouldn't be any volatile components there... but there may be a small amount volatile inclusions scatter through the meteorite. It is not wise to breathe the vapors from "hot" iron... so if the smith is using adequate ventilation and proper procedures..... You may want to be sure you are working with an un-oxidized meteorite. Nantan is and old "fall" and has weathered for 400 years. Most of the pieces will mainly be iron oxides rather than workable metallic iron. Your Smith will know when they go to forge it and it will "fall apart under the hammer." Best of luck and let us know how it goes! ![]() BSMStar |
|
![]() |
![]() |
|
|