Quote:
Originally Posted by asomotif
later than 20th Century... Is the iron still hot ?


Detlef, what do you mean by a blowhole ?

Ps. I can imagine that during forging some flaws may occur and than you can of course decide to make some repair when this occurs in a stage where the product is already near its final form/shape.
But than is looks like the only flaw in this blade.
I really like the shape.

Hello Willem,
sorry for misunderstanding, I've used an online-dictionary. I mean a forge mistake. Maybe a inclusion from cinder. Nearly the same guess as Mr. Maisey mentioned.