Yes Bob, that peened tang would present a problem.

So patch. This jabung mix can be handled with bare hands, you make up the mix, heat it to fluid, then let it cool down until you can pick up a piece that is just warm enough to handle like putty. Roll a little bit, more than sufficient to fill the hole, between your fingers, push it into the hole, then heat up a little piece of steel, something like a nail, grip it with vice grips, and apply the hot steel to the jabung to melt it and let it penetrate the hole. When it is set, but not yet hard, use a bit of sharp wood to cut off the excess, clean up around the fill with mineral turpentine and a hard toothbrush.