View Single Post
Old 11th July 2021, 01:37 PM   #15
kai
Member
 
Join Date: Apr 2005
Posts: 3,219
Default

Quote:
Originally Posted by JBG163 View Post
Seems the two responses are good. The kris shows a harder steel use for the edge (darker because of the better carbon content than the rest) plus the quench line. You can see that variation of the quench line go above the harder edge, especially on the tip
Yes, Julien - the quench is quite extensive and tends to extend past the steel layer.

Regards,
Kai
kai is offline   Reply With Quote