NB:- my mention of hydrochloric acid was only for spotting, not ever for a soak, and when you spot with the stuff you stay right there and watch it.[/QUOTE]

Alan, I was on the same track as you when you were talking about using acid on the rust...it would be plain bad to put that stuff anywhere but where you'd want it to work.

I have used vinegar to re-etch Moro blades, but never used it as a cleaner as well...I will also have to see if I can find some unsweetened pineapple juice here as well...again, thanks for all your inputs and suggestions...I am grateful.