Quote:
Originally Posted by archer
Very Interesting quite a find The ricasso area pattern looks much bigger than the rest of the blade. Perhaps, it is due to more forge work at the hilt. I'm really liking your progress done without making the blade look over cleaned. Care to share the steps used? Steve
|
have used the process to our friend ARIEL."for the blade, paper body car has used a "water grain 800, and 1200...the blade was in the same State as the handle!
then after the sanding rinse with SOAP or dishwashing liquid with water...dry, degrease the blade with alcohol or acetone.dry.heat hot vinegar and pass it on the blade with a cloth or sponge,neutralize with bicarbonate soude diluted with water about four large spoons to 5 litres hot water...Let it soak for about 5 minutes, rinse has water clear, wipe, dry and lubricate with wd40...