Quote:
Originally Posted by A. G. Maisey
Richard, I attempted to access your pics, but cannot get to them. Some sort of "not a member" thing.

By what you have written it looks as if you smelted the meteoritic material.

.
Yes indeed I did melt it...its my "thing".
I used Nantan meteorite from China and it has 6-7% nickel...the color tone from 7% is not too different from 2% so I diluted it to 2% with iron and added enough carbon to bring it to about 0.6%...thus making an ingot of good steel.

Sorry about not being able to access Don Fogg's discussion site...I need to place all that on my website...its on the list of things to do.

I never found the folding in the raw meteorite all that efficient...with some space rocks its not possible as they are too full of crud to work in that fassion....BUT...that is more traditional.

Ric