Hi,
I have had similar experience and I tried "Adding" magnetic property to a hand forged dagger. I had used an old file for forging the dagger. After Forging, Initial grinding and heat treat ment, I honed it with carborundum stone (400-450 grit) with hand. Blade size was about 8.5 inches, and 1.5 inches wide. I honned it for about 12 hours in a span of one month.
It developed strong magnetic property in the center of the blade. I have not checked the calibration though but similar method did not worked on the blades forged from Leaf Srpings.