I have seen many katar with scarf welded homogeneous steel tips that were heat treated. In those cases it added strength to this area. Haven't seen this on tulwar which makes this one likely a repair. However, the smith was knowledgeable of wootz as they managed the repair carefully, because you don't see much faded pattern at the join which would have required careful control of the heat.